Steel AISI 02
C 0,9 %
Mn 2,0 %
Cr 0,4 %
V 0,1 %
High degree of dimensional stability retains its cutting properties, resistant to wear
Applicability
Manufacture of jigs, gauges, dies, templates, rules, blanking tools, measuring instruments, precision parts and guide slide rails
Supply, soft annealed, max. 229 HB (max. 770 N/mm2)
Heat Treatment Data Stress-relief annealing 650 - 680 °C
Soft annealing 680 - 720 °C Hardening 780 - 800 °C
Quenching Oil or warm bath Tempering 180 - 200 °C
Refroidissement Huile ou bain chaud Revenu 180 - 200 °C